某钛铁矿选矿工艺探索研究
DOI:
作者:
作者单位:

作者简介:

通讯作者:

中图分类号:

TD952

基金项目:


Research on mineral processing technology for an ilmenite ore
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    某地钛铁矿的嵌布粒度不均匀、脉石矿物角闪石因含钛铁矿或磁铁矿包裹体而磁性增强,钛的理论回收率仅65,左右.针对该矿的矿石性质,采用阶段磨矿阶段选别的工艺回收钛铁矿,即将原矿磨至53.37,-0.074 mm后,采用一粗一精强磁选获得钛粗精矿,粗精矿再磨至80,-0.074 mm后经二次强磁精选,一次中磁选脱铁.在原矿TiO2品位7.93,时,获得钛精矿TiO2品位48.10,、回收率45.82,的指标.

    Abstract:

    An ilmenite ore possesses the following properties :dissemination size of ilmenite is uneven ;the magnetism of gangue mineral hornblende is enhanced by ilmenite or magnetite inclusions in it ;the theoreti‐cal recovery rate of TiO2 is only about 65, .In view of these properties ,the stage grinding and the stage separation were used to recycle ilmenite .First ,the rough titanium concentrate was gained by one roughing and one cleaning for high‐intensity magnetic separation after the crude ore was grinded to 53 .37, -0 .074 mm .Then ,iron was removed via the second high‐magnetic separation and one medium‐magnetic separation after the rough ilmenite concentrate was grinded to 80, -0 .074mm .When the TiO2 grade of crude ore was 7 .93, ,ilmenite concentrate was obtained with TiO2 grade of 48 .10, and recovery of 45 .82, .

    参考文献
    相似文献
    引证文献
引用本文

周晓彤,邓丽红,李英霞.某钛铁矿选矿工艺探索研究[J].材料研究与应用,2014,(4).

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2020-04-26
  • 出版日期:
文章二维码
材料研究与应用 ® 2024 版权所有